Advanced search options

Advanced Search Options 🞨

Browse by author name (“Author name starts with…”).

Find ETDs with:

in
/  
in
/  
in
/  
in

Written in Published in Earliest date Latest date

Sorted by

Results per page:

Sorted by: relevance · author · university · dateNew search

You searched for subject:(superalloys). Showing records 1 – 30 of 157 total matches.

[1] [2] [3] [4] [5] [6]

Search Limiters

Last 2 Years | English Only

Degrees

Levels

Languages

Country

▼ Search Limiters

1. Handa, Sukhdeep Singh. Precipitation of Carbides in a Ni-based Superalloy.

Degree: Division of Manufacturing Processes, 2014, University West

  Alloy B is relatively new precipitation hardening superalloy. It´s applications are in the hot sections of the aero engines, rocket nozzles, gas turbines and… (more)

Subjects/Keywords: Carbides; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Handa, S. S. (2014). Precipitation of Carbides in a Ni-based Superalloy. (Thesis). University West. Retrieved from http://urn.kb.se/resolve?urn=urn:nbn:se:hv:diva-6867

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Handa, Sukhdeep Singh. “Precipitation of Carbides in a Ni-based Superalloy.” 2014. Thesis, University West. Accessed December 03, 2020. http://urn.kb.se/resolve?urn=urn:nbn:se:hv:diva-6867.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Handa, Sukhdeep Singh. “Precipitation of Carbides in a Ni-based Superalloy.” 2014. Web. 03 Dec 2020.

Vancouver:

Handa SS. Precipitation of Carbides in a Ni-based Superalloy. [Internet] [Thesis]. University West; 2014. [cited 2020 Dec 03]. Available from: http://urn.kb.se/resolve?urn=urn:nbn:se:hv:diva-6867.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Handa SS. Precipitation of Carbides in a Ni-based Superalloy. [Thesis]. University West; 2014. Available from: http://urn.kb.se/resolve?urn=urn:nbn:se:hv:diva-6867

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

2. Aba-Perea, Pierre-Emmanuel Benjamin. In-situ stress relaxation studies in nickel-base superalloy forgings.

Degree: 2017, University of Manchester

 The manufacturing of nickel-base superalloy forging for aero-engine applications requires a number of thermo-mechanical processing steps, which generate significant residual stresses that can result in… (more)

Subjects/Keywords: Residual stresses; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Aba-Perea, P. B. (2017). In-situ stress relaxation studies in nickel-base superalloy forgings. (Doctoral Dissertation). University of Manchester. Retrieved from http://www.manchester.ac.uk/escholar/uk-ac-man-scw:307034

Chicago Manual of Style (16th Edition):

Aba-Perea, Pierre-Emmanuel Benjamin. “In-situ stress relaxation studies in nickel-base superalloy forgings.” 2017. Doctoral Dissertation, University of Manchester. Accessed December 03, 2020. http://www.manchester.ac.uk/escholar/uk-ac-man-scw:307034.

MLA Handbook (7th Edition):

Aba-Perea, Pierre-Emmanuel Benjamin. “In-situ stress relaxation studies in nickel-base superalloy forgings.” 2017. Web. 03 Dec 2020.

Vancouver:

Aba-Perea PB. In-situ stress relaxation studies in nickel-base superalloy forgings. [Internet] [Doctoral dissertation]. University of Manchester; 2017. [cited 2020 Dec 03]. Available from: http://www.manchester.ac.uk/escholar/uk-ac-man-scw:307034.

Council of Science Editors:

Aba-Perea PB. In-situ stress relaxation studies in nickel-base superalloy forgings. [Doctoral Dissertation]. University of Manchester; 2017. Available from: http://www.manchester.ac.uk/escholar/uk-ac-man-scw:307034


Dalhousie University

3. Murray, Donald Clark. On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy.

Degree: Master of Applied Science, Department of Process Engineering and Applied Science, 2012, Dalhousie University

 Nickel-based Superalloys are widely used in the steam turbine power generation and aerospace industries. They possess the desirable qualities of high-temperature strength, oxidation and corrosion… (more)

Subjects/Keywords: Superalloys; Powder Metallurgy; Oxidation

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Murray, D. C. (2012). On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy. (Masters Thesis). Dalhousie University. Retrieved from http://hdl.handle.net/10222/15246

Chicago Manual of Style (16th Edition):

Murray, Donald Clark. “On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy.” 2012. Masters Thesis, Dalhousie University. Accessed December 03, 2020. http://hdl.handle.net/10222/15246.

MLA Handbook (7th Edition):

Murray, Donald Clark. “On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy.” 2012. Web. 03 Dec 2020.

Vancouver:

Murray DC. On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy. [Internet] [Masters thesis]. Dalhousie University; 2012. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/10222/15246.

Council of Science Editors:

Murray DC. On Improving The Oxidation Resistance Of A Nickel-Based Superalloy Produced By Powder Metallurgy. [Masters Thesis]. Dalhousie University; 2012. Available from: http://hdl.handle.net/10222/15246


University of Manitoba

4. Balachander, Mettupalayam. Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy.

Degree: Mechanical and Manufacturing Engineering, 2010, University of Manitoba

 This research focuses on studying the microstructure of alloy 909, its susceptibility to oxidation at elevated temperatures (~700°C) and substrate coatings compatibility with high velocity… (more)

Subjects/Keywords: Alloy 909; Low CTE; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Balachander, M. (2010). Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy. (Thesis). University of Manitoba. Retrieved from http://hdl.handle.net/1993/4292

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Balachander, Mettupalayam. “Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy.” 2010. Thesis, University of Manitoba. Accessed December 03, 2020. http://hdl.handle.net/1993/4292.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Balachander, Mettupalayam. “Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy.” 2010. Web. 03 Dec 2020.

Vancouver:

Balachander M. Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy. [Internet] [Thesis]. University of Manitoba; 2010. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/1993/4292.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Balachander M. Microstructural characterization and thermal fatigue study of a coated Incoloy 909 Superalloy. [Thesis]. University of Manitoba; 2010. Available from: http://hdl.handle.net/1993/4292

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


University of Manitoba

5. Heggadadevanapura Thammaiah, Mallikarjuna. Isothermal oxidation comparison of three Ni-based superalloys.

Degree: Mechanical Engineering, 2016, University of Manitoba

 Ni-based superalloys are used for high-temperature components of gas turbines in both industrial and aerospace applications due to their ability to maintain dimensional stability under… (more)

Subjects/Keywords: Nickel superalloys; Oxidation; Oxides; Thermodynamics

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Heggadadevanapura Thammaiah, M. (2016). Isothermal oxidation comparison of three Ni-based superalloys. (Masters Thesis). University of Manitoba. Retrieved from http://hdl.handle.net/1993/31594

Chicago Manual of Style (16th Edition):

Heggadadevanapura Thammaiah, Mallikarjuna. “Isothermal oxidation comparison of three Ni-based superalloys.” 2016. Masters Thesis, University of Manitoba. Accessed December 03, 2020. http://hdl.handle.net/1993/31594.

MLA Handbook (7th Edition):

Heggadadevanapura Thammaiah, Mallikarjuna. “Isothermal oxidation comparison of three Ni-based superalloys.” 2016. Web. 03 Dec 2020.

Vancouver:

Heggadadevanapura Thammaiah M. Isothermal oxidation comparison of three Ni-based superalloys. [Internet] [Masters thesis]. University of Manitoba; 2016. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/1993/31594.

Council of Science Editors:

Heggadadevanapura Thammaiah M. Isothermal oxidation comparison of three Ni-based superalloys. [Masters Thesis]. University of Manitoba; 2016. Available from: http://hdl.handle.net/1993/31594

6. Aba-Perea, Pierre-Emmanuel. In-situ stress relaxation studies in nickel-base superalloy forgings.

Degree: PhD, 2017, University of Manchester

 The manufacturing of nickel-base superalloy forging for aero-engine applications requires a number of thermo-mechanical processing steps, which generate significant residual stresses that can result in… (more)

Subjects/Keywords: 620.1; Residual stresses; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Aba-Perea, P. (2017). In-situ stress relaxation studies in nickel-base superalloy forgings. (Doctoral Dissertation). University of Manchester. Retrieved from https://www.research.manchester.ac.uk/portal/en/theses/insitu-stress-relaxation-studies-in-nickelbase-superalloy-forgings(13c9a3e7-8ad3-4d9f-abb3-4e379745318a).html ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.728256

Chicago Manual of Style (16th Edition):

Aba-Perea, Pierre-Emmanuel. “In-situ stress relaxation studies in nickel-base superalloy forgings.” 2017. Doctoral Dissertation, University of Manchester. Accessed December 03, 2020. https://www.research.manchester.ac.uk/portal/en/theses/insitu-stress-relaxation-studies-in-nickelbase-superalloy-forgings(13c9a3e7-8ad3-4d9f-abb3-4e379745318a).html ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.728256.

MLA Handbook (7th Edition):

Aba-Perea, Pierre-Emmanuel. “In-situ stress relaxation studies in nickel-base superalloy forgings.” 2017. Web. 03 Dec 2020.

Vancouver:

Aba-Perea P. In-situ stress relaxation studies in nickel-base superalloy forgings. [Internet] [Doctoral dissertation]. University of Manchester; 2017. [cited 2020 Dec 03]. Available from: https://www.research.manchester.ac.uk/portal/en/theses/insitu-stress-relaxation-studies-in-nickelbase-superalloy-forgings(13c9a3e7-8ad3-4d9f-abb3-4e379745318a).html ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.728256.

Council of Science Editors:

Aba-Perea P. In-situ stress relaxation studies in nickel-base superalloy forgings. [Doctoral Dissertation]. University of Manchester; 2017. Available from: https://www.research.manchester.ac.uk/portal/en/theses/insitu-stress-relaxation-studies-in-nickelbase-superalloy-forgings(13c9a3e7-8ad3-4d9f-abb3-4e379745318a).html ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.728256

7. Wang, Anbo. Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres.

Degree: PhD, 2018, Worcester Polytechnic Institute

 The heat-treating industry is in need of heat- treatment furnace materials and fixtures that have a long service life and reduced heat capacity. Based on… (more)

Subjects/Keywords: superalloys; aluminizing; inter-metallics; carburi

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Wang, A. (2018). Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres. (Doctoral Dissertation). Worcester Polytechnic Institute. Retrieved from etd-011218-224945 ; https://digitalcommons.wpi.edu/etd-dissertations/24

Chicago Manual of Style (16th Edition):

Wang, Anbo. “Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres.” 2018. Doctoral Dissertation, Worcester Polytechnic Institute. Accessed December 03, 2020. etd-011218-224945 ; https://digitalcommons.wpi.edu/etd-dissertations/24.

MLA Handbook (7th Edition):

Wang, Anbo. “Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres.” 2018. Web. 03 Dec 2020.

Vancouver:

Wang A. Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres. [Internet] [Doctoral dissertation]. Worcester Polytechnic Institute; 2018. [cited 2020 Dec 03]. Available from: etd-011218-224945 ; https://digitalcommons.wpi.edu/etd-dissertations/24.

Council of Science Editors:

Wang A. Life Extension of High Temperature Structural Alloys by Surface Engineering in Gas and Vacuum Carburizing Atmospheres. [Doctoral Dissertation]. Worcester Polytechnic Institute; 2018. Available from: etd-011218-224945 ; https://digitalcommons.wpi.edu/etd-dissertations/24


University of Florida

8. Mullenix, Lindsay J. Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines.

Degree: PhD, Materials Science and Engineering, 2018, University of Florida

 Single crystal nickel based superalloys have gained popularity for use in turbine blades in the first few rows of the hot section in industrial gas… (more)

Subjects/Keywords: creep  – microstructure  – nickel  – superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Mullenix, L. J. (2018). Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines. (Doctoral Dissertation). University of Florida. Retrieved from https://ufdc.ufl.edu/UFE0051458

Chicago Manual of Style (16th Edition):

Mullenix, Lindsay J. “Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines.” 2018. Doctoral Dissertation, University of Florida. Accessed December 03, 2020. https://ufdc.ufl.edu/UFE0051458.

MLA Handbook (7th Edition):

Mullenix, Lindsay J. “Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines.” 2018. Web. 03 Dec 2020.

Vancouver:

Mullenix LJ. Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines. [Internet] [Doctoral dissertation]. University of Florida; 2018. [cited 2020 Dec 03]. Available from: https://ufdc.ufl.edu/UFE0051458.

Council of Science Editors:

Mullenix LJ. Evaluation of Solution Heat Treatment and Creep Properties of CMSX-8 B/C for Industrial Gas Turbines. [Doctoral Dissertation]. University of Florida; 2018. Available from: https://ufdc.ufl.edu/UFE0051458

9. Thébaud, Louis. Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™.

Degree: Docteur es, Mécanique des solides, des matériaux, des structures et des surfaces, 2017, Chasseneuil-du-Poitou, Ecole nationale supérieure de mécanique et d'aérotechnique

Compte tenu de l’évolution des températures d’entrée de turbines, le principal enjeu pour les métallurgistes est d’élaborer des alliages capables de présenter d’excellentes propriétés mécaniques… (more)

Subjects/Keywords: Superalliage base nickel; Ni-based superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Thébaud, L. (2017). Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™. (Doctoral Dissertation). Chasseneuil-du-Poitou, Ecole nationale supérieure de mécanique et d'aérotechnique. Retrieved from http://www.theses.fr/2017ESMA0033

Chicago Manual of Style (16th Edition):

Thébaud, Louis. “Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™.” 2017. Doctoral Dissertation, Chasseneuil-du-Poitou, Ecole nationale supérieure de mécanique et d'aérotechnique. Accessed December 03, 2020. http://www.theses.fr/2017ESMA0033.

MLA Handbook (7th Edition):

Thébaud, Louis. “Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™.” 2017. Web. 03 Dec 2020.

Vancouver:

Thébaud L. Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™. [Internet] [Doctoral dissertation]. Chasseneuil-du-Poitou, Ecole nationale supérieure de mécanique et d'aérotechnique; 2017. [cited 2020 Dec 03]. Available from: http://www.theses.fr/2017ESMA0033.

Council of Science Editors:

Thébaud L. Etude des relations entre microstructure et propriétés mécaniques du nouveau superalliage base nickel AD730™ : Relationships Between Microstructural Parameters and Mechanical Properties of a new Nickel Based Superalloy AD730™. [Doctoral Dissertation]. Chasseneuil-du-Poitou, Ecole nationale supérieure de mécanique et d'aérotechnique; 2017. Available from: http://www.theses.fr/2017ESMA0033

10. Rhein, Robert Karl. Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys.

Degree: 2019, University of California – eScholarship, University of California

 L12-containing Co-base superalloys are of significant interest due to their high temperature strength and oxidation resistance. Previous research has shown that this class of alloys… (more)

Subjects/Keywords: Materials Science; High-temperature materials; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Rhein, R. K. (2019). Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys. (Thesis). University of California – eScholarship, University of California. Retrieved from http://www.escholarship.org/uc/item/61s3k0nx

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Rhein, Robert Karl. “Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys.” 2019. Thesis, University of California – eScholarship, University of California. Accessed December 03, 2020. http://www.escholarship.org/uc/item/61s3k0nx.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Rhein, Robert Karl. “Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys.” 2019. Web. 03 Dec 2020.

Vancouver:

Rhein RK. Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys. [Internet] [Thesis]. University of California – eScholarship, University of California; 2019. [cited 2020 Dec 03]. Available from: http://www.escholarship.org/uc/item/61s3k0nx.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Rhein RK. Thermodynamics and Creep Behavior of L12-containing Co-base Superalloys. [Thesis]. University of California – eScholarship, University of California; 2019. Available from: http://www.escholarship.org/uc/item/61s3k0nx

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


University of Illinois – Urbana-Champaign

11. Emigh, Megan Genevieve. The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys.

Degree: PhD, Materials Science & Engr, 2018, University of Illinois – Urbana-Champaign

Superalloys have often been used for applications where a metal that can withstand high stresses, retain high strength at high temperatures, and resist oxidization is… (more)

Subjects/Keywords: Superalloys; Precipitates; Nanotwins; Aging; Sputter Deposition

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Emigh, M. G. (2018). The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys. (Doctoral Dissertation). University of Illinois – Urbana-Champaign. Retrieved from http://hdl.handle.net/2142/102442

Chicago Manual of Style (16th Edition):

Emigh, Megan Genevieve. “The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys.” 2018. Doctoral Dissertation, University of Illinois – Urbana-Champaign. Accessed December 03, 2020. http://hdl.handle.net/2142/102442.

MLA Handbook (7th Edition):

Emigh, Megan Genevieve. “The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys.” 2018. Web. 03 Dec 2020.

Vancouver:

Emigh MG. The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys. [Internet] [Doctoral dissertation]. University of Illinois – Urbana-Champaign; 2018. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/2142/102442.

Council of Science Editors:

Emigh MG. The influence of mixed hexagonal close-packed and face-centered cubic ordering on precipitation pathways and kinetics in sputtered superalloys. [Doctoral Dissertation]. University of Illinois – Urbana-Champaign; 2018. Available from: http://hdl.handle.net/2142/102442


University of British Columbia

12. Li, Ting. Banding in nickel-base superalloys and steels.

Degree: Master of Applied Science - MASc, Materials Engineering, 2007, University of British Columbia

 Process irregularities in remelting furnace operation have an impact on the ingot solidification structure which depends on the local thermal conditions and the alloy concerned.… (more)

Subjects/Keywords: banding; superalloys; steels

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Li, T. (2007). Banding in nickel-base superalloys and steels. (Masters Thesis). University of British Columbia. Retrieved from http://hdl.handle.net/2429/344

Chicago Manual of Style (16th Edition):

Li, Ting. “Banding in nickel-base superalloys and steels.” 2007. Masters Thesis, University of British Columbia. Accessed December 03, 2020. http://hdl.handle.net/2429/344.

MLA Handbook (7th Edition):

Li, Ting. “Banding in nickel-base superalloys and steels.” 2007. Web. 03 Dec 2020.

Vancouver:

Li T. Banding in nickel-base superalloys and steels. [Internet] [Masters thesis]. University of British Columbia; 2007. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/2429/344.

Council of Science Editors:

Li T. Banding in nickel-base superalloys and steels. [Masters Thesis]. University of British Columbia; 2007. Available from: http://hdl.handle.net/2429/344


Brno University of Technology

13. Fukátková, Pavla. Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys.

Degree: 2018, Brno University of Technology

 This thesis is focused on changes of microstructure of nickel - base superalloys (alloy ZH6K) from the point of view of quantitative and qualitative classification.… (more)

Subjects/Keywords: Niklové superslitiny; žáruvzdorné a žárupevné vlastnosti; chemické složení superslitin; mikrostruktura superslitin; Nickel - base superalloys; heat-resisting and creepresisting properties; chemist of superalloys; microstrukture of superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Fukátková, P. (2018). Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys. (Thesis). Brno University of Technology. Retrieved from http://hdl.handle.net/11012/64089

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Fukátková, Pavla. “Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys.” 2018. Thesis, Brno University of Technology. Accessed December 03, 2020. http://hdl.handle.net/11012/64089.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Fukátková, Pavla. “Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys.” 2018. Web. 03 Dec 2020.

Vancouver:

Fukátková P. Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys. [Internet] [Thesis]. Brno University of Technology; 2018. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/11012/64089.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Fukátková P. Struktura a vlastnosti litých niklových superslitin: Structure and Properties of Cast Nickel-base Superalloys. [Thesis]. Brno University of Technology; 2018. Available from: http://hdl.handle.net/11012/64089

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


Indian Institute of Science

14. Vinay, K S. Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys.

Degree: MSc Engg, Engineering, 2018, Indian Institute of Science

 Nickel based superalloys are high temperature materials which find application as blade and disc components of jet engines due to their ability to retain their… (more)

Subjects/Keywords: Nickel Based Superalloys; Solidification Alloys; Alloy Composition; Ni-Based Superalloys; Ni-Al-Re/Ru Alloys; Materials Engineering

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Vinay, K. S. (2018). Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys. (Masters Thesis). Indian Institute of Science. Retrieved from http://etd.iisc.ac.in/handle/2005/4056

Chicago Manual of Style (16th Edition):

Vinay, K S. “Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys.” 2018. Masters Thesis, Indian Institute of Science. Accessed December 03, 2020. http://etd.iisc.ac.in/handle/2005/4056.

MLA Handbook (7th Edition):

Vinay, K S. “Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys.” 2018. Web. 03 Dec 2020.

Vancouver:

Vinay KS. Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys. [Internet] [Masters thesis]. Indian Institute of Science; 2018. [cited 2020 Dec 03]. Available from: http://etd.iisc.ac.in/handle/2005/4056.

Council of Science Editors:

Vinay KS. Microstructural Evolution of Directionally Solidified Ni-Al-Re/Ru Alloys. [Masters Thesis]. Indian Institute of Science; 2018. Available from: http://etd.iisc.ac.in/handle/2005/4056


Penn State University

15. Kim, DongEung. THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES.

Degree: 2011, Penn State University

 A computational prediction of materials performance is becoming increasingly important for the development of new materials. In the case of multicomponent materials such as Ni… (more)

Subjects/Keywords: thermodynamic modeling; Ni-base superalloys; elastic property; thermal expansion property

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Kim, D. (2011). THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES. (Thesis). Penn State University. Retrieved from https://submit-etda.libraries.psu.edu/catalog/12437

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Kim, DongEung. “THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES.” 2011. Thesis, Penn State University. Accessed December 03, 2020. https://submit-etda.libraries.psu.edu/catalog/12437.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Kim, DongEung. “THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES.” 2011. Web. 03 Dec 2020.

Vancouver:

Kim D. THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES. [Internet] [Thesis]. Penn State University; 2011. [cited 2020 Dec 03]. Available from: https://submit-etda.libraries.psu.edu/catalog/12437.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Kim D. THERMODYNAMIC MODELING AND PREDICTION OF ELASTIC AND THERMAL EXPANSION PROPERTIES OF NI-BASE SUPERALLOYS: APPLICATION TO NI-AL-PT-CR-HF SYSTEM WITH γ AND γ' PHASES. [Thesis]. Penn State University; 2011. Available from: https://submit-etda.libraries.psu.edu/catalog/12437

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


Penn State University

16. Ross, Austin Joseph. Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures.

Degree: 2015, Penn State University

 This thesis will focus on the formation of a protective α-Al2O3 layer on Ni-base superalloys during high temperature oxidation in dry and wet gaseous environments.… (more)

Subjects/Keywords: High Temperature Oxidation; Ni-Base superalloys; Selective Oxidation; Al2O3 Scale

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Ross, A. J. (2015). Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures. (Thesis). Penn State University. Retrieved from https://submit-etda.libraries.psu.edu/catalog/26535

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Ross, Austin Joseph. “Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures.” 2015. Thesis, Penn State University. Accessed December 03, 2020. https://submit-etda.libraries.psu.edu/catalog/26535.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Ross, Austin Joseph. “Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures.” 2015. Web. 03 Dec 2020.

Vancouver:

Ross AJ. Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures. [Internet] [Thesis]. Penn State University; 2015. [cited 2020 Dec 03]. Available from: https://submit-etda.libraries.psu.edu/catalog/26535.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Ross AJ. Solubility of Oxygen and Hydrogen and Diffusivity of Oxygen in the fcc Phase of the Al-fe-ni-h-o System with Application to the Formation of a Protective α-al2o3 Scale at High Temperatures. [Thesis]. Penn State University; 2015. Available from: https://submit-etda.libraries.psu.edu/catalog/26535

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


Penn State University

17. Ross, Austin Joseph. A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE.

Degree: 2017, Penn State University

 This thesis focuses on the addition of the reactive element Hf to aid in the oxidation resistance of Ni-superalloys. Hf will improve the oxidation resistance… (more)

Subjects/Keywords: Oxidation; Superalloys; Bond-coat; HfO2; Hafnium; external scale; TGO

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Ross, A. J. (2017). A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE. (Thesis). Penn State University. Retrieved from https://submit-etda.libraries.psu.edu/catalog/14808ajr335

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Ross, Austin Joseph. “A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE.” 2017. Thesis, Penn State University. Accessed December 03, 2020. https://submit-etda.libraries.psu.edu/catalog/14808ajr335.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Ross, Austin Joseph. “A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE.” 2017. Web. 03 Dec 2020.

Vancouver:

Ross AJ. A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE. [Internet] [Thesis]. Penn State University; 2017. [cited 2020 Dec 03]. Available from: https://submit-etda.libraries.psu.edu/catalog/14808ajr335.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Ross AJ. A THERMODYNAMICS BASED GUIDE TO ADDING HF TO A NI-SUPERALLOY TO IMPROVE OXIDATION RESISTANCE. [Thesis]. Penn State University; 2017. Available from: https://submit-etda.libraries.psu.edu/catalog/14808ajr335

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


Carnegie Mellon University

18. Harrison, Ryan K.S. Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants.

Degree: 2018, Carnegie Mellon University

 The analysis of microstructural shapes is an underutilized tool in the field of materials science. Typical observations of morphology are qualitative, rather than quantitative, which… (more)

Subjects/Keywords: Additive manufacturing; Cell biology; Moment invariants; Morphology; Shape analysis; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Harrison, R. K. S. (2018). Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants. (Thesis). Carnegie Mellon University. Retrieved from http://repository.cmu.edu/dissertations/1162

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Harrison, Ryan K S. “Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants.” 2018. Thesis, Carnegie Mellon University. Accessed December 03, 2020. http://repository.cmu.edu/dissertations/1162.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Harrison, Ryan K S. “Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants.” 2018. Web. 03 Dec 2020.

Vancouver:

Harrison RKS. Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants. [Internet] [Thesis]. Carnegie Mellon University; 2018. [cited 2020 Dec 03]. Available from: http://repository.cmu.edu/dissertations/1162.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Harrison RKS. Investigating the Relationships Between Material Properties and Microstructural Shapes as Quantified by Moment Invariants. [Thesis]. Carnegie Mellon University; 2018. Available from: http://repository.cmu.edu/dissertations/1162

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


University of Manitoba

19. Adebajo, Olaniyi. Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy.

Degree: Mechanical Engineering, 2016, University of Manitoba

 Transient Liquid phase bonding (TLP) has evolved as a viable method of joining difficult-to-weld superalloys with potential of producing joints with comparable mechanical properties to… (more)

Subjects/Keywords: Transient Liquid Phase Bonding; Corrosion; Superalloys; Potentiodynamic Polarization

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Adebajo, O. (2016). Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy. (Masters Thesis). University of Manitoba. Retrieved from http://hdl.handle.net/1993/31165

Chicago Manual of Style (16th Edition):

Adebajo, Olaniyi. “Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy.” 2016. Masters Thesis, University of Manitoba. Accessed December 03, 2020. http://hdl.handle.net/1993/31165.

MLA Handbook (7th Edition):

Adebajo, Olaniyi. “Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy.” 2016. Web. 03 Dec 2020.

Vancouver:

Adebajo O. Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy. [Internet] [Masters thesis]. University of Manitoba; 2016. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/1993/31165.

Council of Science Editors:

Adebajo O. Effects of transient liquid phase bonding on corrosion performance of a single crystal aerospace superalloy. [Masters Thesis]. University of Manitoba; 2016. Available from: http://hdl.handle.net/1993/31165

20. Rettberg, Luke. Rejuvenation of Ni-base Superalloys GTD444 and René N5.

Degree: 2016, University of California – eScholarship, University of California

 During service, superalloy turbine components degrade over time by creep and fatigue deformation mechanisms due to a complex combination of stresses at high temperatures. Service… (more)

Subjects/Keywords: Materials Science; Creep; Fatigue; Recrystallization; Rejuvenation; Resonant Ultrasound Spectroscopy; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Rettberg, L. (2016). Rejuvenation of Ni-base Superalloys GTD444 and René N5. (Thesis). University of California – eScholarship, University of California. Retrieved from http://www.escholarship.org/uc/item/31n72339

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Chicago Manual of Style (16th Edition):

Rettberg, Luke. “Rejuvenation of Ni-base Superalloys GTD444 and René N5.” 2016. Thesis, University of California – eScholarship, University of California. Accessed December 03, 2020. http://www.escholarship.org/uc/item/31n72339.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

MLA Handbook (7th Edition):

Rettberg, Luke. “Rejuvenation of Ni-base Superalloys GTD444 and René N5.” 2016. Web. 03 Dec 2020.

Vancouver:

Rettberg L. Rejuvenation of Ni-base Superalloys GTD444 and René N5. [Internet] [Thesis]. University of California – eScholarship, University of California; 2016. [cited 2020 Dec 03]. Available from: http://www.escholarship.org/uc/item/31n72339.

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation

Council of Science Editors:

Rettberg L. Rejuvenation of Ni-base Superalloys GTD444 and René N5. [Thesis]. University of California – eScholarship, University of California; 2016. Available from: http://www.escholarship.org/uc/item/31n72339

Note: this citation may be lacking information needed for this citation format:
Not specified: Masters Thesis or Doctoral Dissertation


University of Sheffield

21. Hanna, Muayyad Dawood. The formation of platinum aluminide coatings on IN-738 and their oxidation resistance.

Degree: PhD, 1982, University of Sheffield

 Platinum alumnide coatings have been produced by first plating a thin layer of platinum usinq a fused salt platinum plating technique and then pack aluminizing… (more)

Subjects/Keywords: 669; Nickel-based superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Hanna, M. D. (1982). The formation of platinum aluminide coatings on IN-738 and their oxidation resistance. (Doctoral Dissertation). University of Sheffield. Retrieved from http://etheses.whiterose.ac.uk/2946/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.280551

Chicago Manual of Style (16th Edition):

Hanna, Muayyad Dawood. “The formation of platinum aluminide coatings on IN-738 and their oxidation resistance.” 1982. Doctoral Dissertation, University of Sheffield. Accessed December 03, 2020. http://etheses.whiterose.ac.uk/2946/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.280551.

MLA Handbook (7th Edition):

Hanna, Muayyad Dawood. “The formation of platinum aluminide coatings on IN-738 and their oxidation resistance.” 1982. Web. 03 Dec 2020.

Vancouver:

Hanna MD. The formation of platinum aluminide coatings on IN-738 and their oxidation resistance. [Internet] [Doctoral dissertation]. University of Sheffield; 1982. [cited 2020 Dec 03]. Available from: http://etheses.whiterose.ac.uk/2946/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.280551.

Council of Science Editors:

Hanna MD. The formation of platinum aluminide coatings on IN-738 and their oxidation resistance. [Doctoral Dissertation]. University of Sheffield; 1982. Available from: http://etheses.whiterose.ac.uk/2946/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.280551

22. Jones, Robert Edward. Bondcoat developments for thermal barrier coatings.

Degree: PhD, 1999, Sheffield Hallam University

 The prime design considerations for modern nickel based superalloys for use in aero gas-turbine engines, are those of mechanical performance, namely good resistance to creep… (more)

Subjects/Keywords: 620.11223; Nickel based superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Jones, R. E. (1999). Bondcoat developments for thermal barrier coatings. (Doctoral Dissertation). Sheffield Hallam University. Retrieved from http://shura.shu.ac.uk/3137/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.297858

Chicago Manual of Style (16th Edition):

Jones, Robert Edward. “Bondcoat developments for thermal barrier coatings.” 1999. Doctoral Dissertation, Sheffield Hallam University. Accessed December 03, 2020. http://shura.shu.ac.uk/3137/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.297858.

MLA Handbook (7th Edition):

Jones, Robert Edward. “Bondcoat developments for thermal barrier coatings.” 1999. Web. 03 Dec 2020.

Vancouver:

Jones RE. Bondcoat developments for thermal barrier coatings. [Internet] [Doctoral dissertation]. Sheffield Hallam University; 1999. [cited 2020 Dec 03]. Available from: http://shura.shu.ac.uk/3137/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.297858.

Council of Science Editors:

Jones RE. Bondcoat developments for thermal barrier coatings. [Doctoral Dissertation]. Sheffield Hallam University; 1999. Available from: http://shura.shu.ac.uk/3137/ ; http://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.297858

23. Anyanwu, Chidinma. A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys.

Degree: Mechanical Engineering, 2019, University of Manitoba

 Cobalt-based superalloys have been used for several decades in manufacturing various gas turbine engine components because of their excellent high-temperature creep and fatigue strengths and… (more)

Subjects/Keywords: Superalloys; TLP bonding

…Role of alloying elements in cobalt-based superalloys… …9 Table 2.2: Effect alloying elements on γ’-strengthened cobalt-based superalloys… …creep, fatigue, and oxidation among others. For a long time, nickel-based superalloys have… …x5D;–[3]. Nickel-based superalloys gain their good properties at high temperature… …improve on the existing Ni-based superalloys but also to develop new materials to meet future… 

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Anyanwu, C. (2019). A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys. (Masters Thesis). University of Manitoba. Retrieved from http://hdl.handle.net/1993/34099

Chicago Manual of Style (16th Edition):

Anyanwu, Chidinma. “A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys.” 2019. Masters Thesis, University of Manitoba. Accessed December 03, 2020. http://hdl.handle.net/1993/34099.

MLA Handbook (7th Edition):

Anyanwu, Chidinma. “A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys.” 2019. Web. 03 Dec 2020.

Vancouver:

Anyanwu C. A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys. [Internet] [Masters thesis]. University of Manitoba; 2019. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/1993/34099.

Council of Science Editors:

Anyanwu C. A comparative study on the transient liquid phase bonding of gamma prime (γ’)-strengthened cobalt- and nickel-based superalloys. [Masters Thesis]. University of Manitoba; 2019. Available from: http://hdl.handle.net/1993/34099


Clemson University

24. Richardson, Boyce. Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys.

Degree: MS, Mechanical Engineering, 2013, Clemson University

 The formation of subsurface damage during machining of nickel-based superalloys is a critical quality concern for the manufacture of gas turbine components. The identification and… (more)

Subjects/Keywords: Image Analysis; Machining Affected Zone; Milling; Nickel-Based Superalloys; Mechanical Engineering

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Richardson, B. (2013). Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys. (Masters Thesis). Clemson University. Retrieved from https://tigerprints.clemson.edu/all_theses/1054

Chicago Manual of Style (16th Edition):

Richardson, Boyce. “Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys.” 2013. Masters Thesis, Clemson University. Accessed December 03, 2020. https://tigerprints.clemson.edu/all_theses/1054.

MLA Handbook (7th Edition):

Richardson, Boyce. “Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys.” 2013. Web. 03 Dec 2020.

Vancouver:

Richardson B. Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys. [Internet] [Masters thesis]. Clemson University; 2013. [cited 2020 Dec 03]. Available from: https://tigerprints.clemson.edu/all_theses/1054.

Council of Science Editors:

Richardson B. Identification of and Effects on the Depth of the Machining Affected Zone in Nickel-Based Superalloys. [Masters Thesis]. Clemson University; 2013. Available from: https://tigerprints.clemson.edu/all_theses/1054


Loughborough University

25. Newman, Scott. Microstructural evolution in coated conventionally cast Ni-based superalloys.

Degree: PhD, 2013, Loughborough University

 The aim of this research project was to investigate the microstructural changes of MCrAlY coated Ni-based superalloys that are routinely used in industrial gas turbine… (more)

Subjects/Keywords: 620.1; Ni-based superalloys; High temperature coatings; MCrAlY; Thermal Barrier coating

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Newman, S. (2013). Microstructural evolution in coated conventionally cast Ni-based superalloys. (Doctoral Dissertation). Loughborough University. Retrieved from http://hdl.handle.net/2134/12468

Chicago Manual of Style (16th Edition):

Newman, Scott. “Microstructural evolution in coated conventionally cast Ni-based superalloys.” 2013. Doctoral Dissertation, Loughborough University. Accessed December 03, 2020. http://hdl.handle.net/2134/12468.

MLA Handbook (7th Edition):

Newman, Scott. “Microstructural evolution in coated conventionally cast Ni-based superalloys.” 2013. Web. 03 Dec 2020.

Vancouver:

Newman S. Microstructural evolution in coated conventionally cast Ni-based superalloys. [Internet] [Doctoral dissertation]. Loughborough University; 2013. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/2134/12468.

Council of Science Editors:

Newman S. Microstructural evolution in coated conventionally cast Ni-based superalloys. [Doctoral Dissertation]. Loughborough University; 2013. Available from: http://hdl.handle.net/2134/12468


University of South Carolina

26. Hrutkay, Kyle. Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures.

Degree: MS, Nuclear Engineering, 2013, University of South Carolina

  Haynes 230 and Inconel 617 are austenitic nickel based superalloys, which are candidate structural materials for next generation high temperature nuclear reactors. High temperature… (more)

Subjects/Keywords: Engineering; Nuclear Engineering; Dynamic Strain Ageing; Microstructure; Recrystallization; Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Hrutkay, K. (2013). Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures. (Masters Thesis). University of South Carolina. Retrieved from https://scholarcommons.sc.edu/etd/2365

Chicago Manual of Style (16th Edition):

Hrutkay, Kyle. “Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures.” 2013. Masters Thesis, University of South Carolina. Accessed December 03, 2020. https://scholarcommons.sc.edu/etd/2365.

MLA Handbook (7th Edition):

Hrutkay, Kyle. “Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures.” 2013. Web. 03 Dec 2020.

Vancouver:

Hrutkay K. Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures. [Internet] [Masters thesis]. University of South Carolina; 2013. [cited 2020 Dec 03]. Available from: https://scholarcommons.sc.edu/etd/2365.

Council of Science Editors:

Hrutkay K. Evolution of Microstructure of Haynes 230 and Inconel 617 Under Mechanical Testing At High Temperatures. [Masters Thesis]. University of South Carolina; 2013. Available from: https://scholarcommons.sc.edu/etd/2365

27. Vultos, Winnie. Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy.

Degree: Docteur es, Sciences et génie des matériaux, 2019, Université Toulouse III – Paul Sabatier

L'étude menée au cours de ce travail de thèse consiste à analyser les micromécanismes qui contrôlent la déformation en fluage à 700°C, dans le superalliage… (more)

Subjects/Keywords: Fluage; Mécanismes; Superalliages; Déformation; MET; Creep; Mechanisms; Superalloys; Deformation; TEM

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Vultos, W. (2019). Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy. (Doctoral Dissertation). Université Toulouse III – Paul Sabatier. Retrieved from http://www.theses.fr/2019TOU30166

Chicago Manual of Style (16th Edition):

Vultos, Winnie. “Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy.” 2019. Doctoral Dissertation, Université Toulouse III – Paul Sabatier. Accessed December 03, 2020. http://www.theses.fr/2019TOU30166.

MLA Handbook (7th Edition):

Vultos, Winnie. “Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy.” 2019. Web. 03 Dec 2020.

Vancouver:

Vultos W. Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy. [Internet] [Doctoral dissertation]. Université Toulouse III – Paul Sabatier; 2019. [cited 2020 Dec 03]. Available from: http://www.theses.fr/2019TOU30166.

Council of Science Editors:

Vultos W. Influence de la microstructure sur les micromécanismes de déformation en fluage dans le superalliage AD730TM : Influence of the microstructure on creep deformation micromechanisms in the AD730TM superalloy. [Doctoral Dissertation]. Université Toulouse III – Paul Sabatier; 2019. Available from: http://www.theses.fr/2019TOU30166


University of Leicester

28. Zhang, Ruiyao. Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys.

Degree: PhD, 2020, University of Leicester

 Neutron diffraction has become a power tool in studies of multi-phase materials such as Ni-base superalloys, provided that diffraction peak from each phase is distinguishable.… (more)

Subjects/Keywords: Assisted Neutron Diffraction; Gamma Double Prime Phase; Ni-base Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Zhang, R. (2020). Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys. (Doctoral Dissertation). University of Leicester. Retrieved from https://doi.org/10.25392/leicester.data.12666749.v1 ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.811530

Chicago Manual of Style (16th Edition):

Zhang, Ruiyao. “Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys.” 2020. Doctoral Dissertation, University of Leicester. Accessed December 03, 2020. https://doi.org/10.25392/leicester.data.12666749.v1 ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.811530.

MLA Handbook (7th Edition):

Zhang, Ruiyao. “Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys.” 2020. Web. 03 Dec 2020.

Vancouver:

Zhang R. Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys. [Internet] [Doctoral dissertation]. University of Leicester; 2020. [cited 2020 Dec 03]. Available from: https://doi.org/10.25392/leicester.data.12666749.v1 ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.811530.

Council of Science Editors:

Zhang R. Variant selection assisted neutron diffraction study on gamma double prime phase in Ni-base superalloys. [Doctoral Dissertation]. University of Leicester; 2020. Available from: https://doi.org/10.25392/leicester.data.12666749.v1 ; https://ethos.bl.uk/OrderDetails.do?uin=uk.bl.ethos.811530


University of Texas – Austin

29. Lopez, Luis Felipe. Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process.

Degree: MSin Engineering, Mechanical Engineering, 2011, University of Texas – Austin

 Vacuum Arc Remelting (VAR) is a secondary process used for homogenization of high-melting-point and oxygen-sensitive materials such as superalloys and titanium alloys. The VAR process… (more)

Subjects/Keywords: Vacuum Arc Remelting; Superalloys; Titanium alloys; Solidification; Channel segregates

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Lopez, L. F. (2011). Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process. (Masters Thesis). University of Texas – Austin. Retrieved from http://hdl.handle.net/2152/ETD-UT-2011-05-2770

Chicago Manual of Style (16th Edition):

Lopez, Luis Felipe. “Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process.” 2011. Masters Thesis, University of Texas – Austin. Accessed December 03, 2020. http://hdl.handle.net/2152/ETD-UT-2011-05-2770.

MLA Handbook (7th Edition):

Lopez, Luis Felipe. “Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process.” 2011. Web. 03 Dec 2020.

Vancouver:

Lopez LF. Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process. [Internet] [Masters thesis]. University of Texas – Austin; 2011. [cited 2020 Dec 03]. Available from: http://hdl.handle.net/2152/ETD-UT-2011-05-2770.

Council of Science Editors:

Lopez LF. Implementation of a high-fidelity axisymmetric model in a Vacuum Arc Remelting process. [Masters Thesis]. University of Texas – Austin; 2011. Available from: http://hdl.handle.net/2152/ETD-UT-2011-05-2770


Ohio University

30. Rich, Jared W. Assessment and Improvement of Wear in Copper Extrusion Dies.

Degree: MS, Mechanical Engineering (Engineering and Technology), 2013, Ohio University

 The purpose of this work was to develop a die wear model for superalloy tooling used in multi-channel copper tube extrusion and determine the feasibility… (more)

Subjects/Keywords: Engineering; Materials Science; Mechanical Engineering; Metallurgy; Copper Extrusion Dies; Multi Channel Tubing; CVD Coating Nickel Based Superalloys; Copper Extrusion Die Life; Heat Treating CVD Coated Superalloys

Record DetailsSimilar RecordsGoogle PlusoneFacebookTwitterCiteULikeMendeleyreddit

APA · Chicago · MLA · Vancouver · CSE | Export to Zotero / EndNote / Reference Manager

APA (6th Edition):

Rich, J. W. (2013). Assessment and Improvement of Wear in Copper Extrusion Dies. (Masters Thesis). Ohio University. Retrieved from http://rave.ohiolink.edu/etdc/view?acc_num=ohiou1386080178

Chicago Manual of Style (16th Edition):

Rich, Jared W. “Assessment and Improvement of Wear in Copper Extrusion Dies.” 2013. Masters Thesis, Ohio University. Accessed December 03, 2020. http://rave.ohiolink.edu/etdc/view?acc_num=ohiou1386080178.

MLA Handbook (7th Edition):

Rich, Jared W. “Assessment and Improvement of Wear in Copper Extrusion Dies.” 2013. Web. 03 Dec 2020.

Vancouver:

Rich JW. Assessment and Improvement of Wear in Copper Extrusion Dies. [Internet] [Masters thesis]. Ohio University; 2013. [cited 2020 Dec 03]. Available from: http://rave.ohiolink.edu/etdc/view?acc_num=ohiou1386080178.

Council of Science Editors:

Rich JW. Assessment and Improvement of Wear in Copper Extrusion Dies. [Masters Thesis]. Ohio University; 2013. Available from: http://rave.ohiolink.edu/etdc/view?acc_num=ohiou1386080178

[1] [2] [3] [4] [5] [6]

.